After the sewage treatment, putting the wet sludge in which the heavy metal content is extremely low, corrupt and broken straw, bentonite, urea in proportioning according to the certain ratio, mixing well-distributed,...After the sewage treatment, putting the wet sludge in which the heavy metal content is extremely low, corrupt and broken straw, bentonite, urea in proportioning according to the certain ratio, mixing well-distributed, taking the shape of Nitrogen slow-release fertilizers, doing the dynamic bioleaching test by the method of Artificial rainfall simulation, researching the slow-release characteristic, water retention. When the mass ratio of the wet sludge whose water content is 82.5%: bentonite: corrupt and broken straw: urea is 62.5: 12.5: 12.5: 12.5, drip washing the 10g Nitrogen slow-release fertilizers by the 80ml distilled water after 48h, the residue rate of urea is 29.63%; Under the room temperature of 25 ℃, 77%RH, moisture evaporate 46.32% after 60 h. The results demonstrate that the slow-release fertilizer has a good release-effect of nitrogen and water conservation effect. It provides the basic for the development and application of the sewage in the aspect of Nitrogen slow-release fertilizers.展开更多
Produced by the production of sulfuric acid from kaolinite type when the Fe2O3 and metakaolin together constitute the kaolinite type pyrite cinder is a typical industrial solid waste. Only in southern Sichuan China st...Produced by the production of sulfuric acid from kaolinite type when the Fe2O3 and metakaolin together constitute the kaolinite type pyrite cinder is a typical industrial solid waste. Only in southern Sichuan China storage capacity has reached millions of tons, that caused serious impact on ecology and environment in this area. It also caused serious waste of resources. The magnetite concentrate and given priority to with partial kaolinite pyrite cinder tailings that were obtained by grinding and magnetic separation. This experiment studied the relationship composition and particle size with its activity when cinder tailings as cement mixed material. The results show that the particle size of D90 were 88 micron, 56 micron, 40 micron, the activity index were 1.036, 1.068, 1.102. The slag after magnetic separation is a kind of very good activity of cement mixed material. It can make good use of the industrial solid waste.展开更多
By using hydrothermal synthesis method, successively adding tetrabutyl titanate and expandable flake graphite in 40 mL 0.95% NH4Cl solution prepared the nano TiO2/expandable flake graphite, which was then settled in m...By using hydrothermal synthesis method, successively adding tetrabutyl titanate and expandable flake graphite in 40 mL 0.95% NH4Cl solution prepared the nano TiO2/expandable flake graphite, which was then settled in muffle furnace in the expansion of 10 s under 800 ℃ and got nanosized TiO2/expanded graphite. Synthesized that with CoFe2O4 by chemical coprecipitation method finally prepared magnetic nanosized photocatalyst TiO2/expanded graphite. Magnetic nanosized TiO2/expanded graphite was studied on the photodegradation performance of methyl orange solution and the magnetic recovery after the degradation of methyl orange solution. The experiment result showed that in 50 mL 25 mg/L methyl orange solution joined 120 mg loading 50% TiO2 of the expanded graphite, exposed to ultraviolet irradiation for 1 h, the methyl orange decolorization ratio was 90%. When the load of CoFe2O4 in nanosized TiO2/expanded graphite reached 40%, its magnetic recovery efficiency reached 94.3%.展开更多
文摘After the sewage treatment, putting the wet sludge in which the heavy metal content is extremely low, corrupt and broken straw, bentonite, urea in proportioning according to the certain ratio, mixing well-distributed, taking the shape of Nitrogen slow-release fertilizers, doing the dynamic bioleaching test by the method of Artificial rainfall simulation, researching the slow-release characteristic, water retention. When the mass ratio of the wet sludge whose water content is 82.5%: bentonite: corrupt and broken straw: urea is 62.5: 12.5: 12.5: 12.5, drip washing the 10g Nitrogen slow-release fertilizers by the 80ml distilled water after 48h, the residue rate of urea is 29.63%; Under the room temperature of 25 ℃, 77%RH, moisture evaporate 46.32% after 60 h. The results demonstrate that the slow-release fertilizer has a good release-effect of nitrogen and water conservation effect. It provides the basic for the development and application of the sewage in the aspect of Nitrogen slow-release fertilizers.
文摘Produced by the production of sulfuric acid from kaolinite type when the Fe2O3 and metakaolin together constitute the kaolinite type pyrite cinder is a typical industrial solid waste. Only in southern Sichuan China storage capacity has reached millions of tons, that caused serious impact on ecology and environment in this area. It also caused serious waste of resources. The magnetite concentrate and given priority to with partial kaolinite pyrite cinder tailings that were obtained by grinding and magnetic separation. This experiment studied the relationship composition and particle size with its activity when cinder tailings as cement mixed material. The results show that the particle size of D90 were 88 micron, 56 micron, 40 micron, the activity index were 1.036, 1.068, 1.102. The slag after magnetic separation is a kind of very good activity of cement mixed material. It can make good use of the industrial solid waste.
文摘By using hydrothermal synthesis method, successively adding tetrabutyl titanate and expandable flake graphite in 40 mL 0.95% NH4Cl solution prepared the nano TiO2/expandable flake graphite, which was then settled in muffle furnace in the expansion of 10 s under 800 ℃ and got nanosized TiO2/expanded graphite. Synthesized that with CoFe2O4 by chemical coprecipitation method finally prepared magnetic nanosized photocatalyst TiO2/expanded graphite. Magnetic nanosized TiO2/expanded graphite was studied on the photodegradation performance of methyl orange solution and the magnetic recovery after the degradation of methyl orange solution. The experiment result showed that in 50 mL 25 mg/L methyl orange solution joined 120 mg loading 50% TiO2 of the expanded graphite, exposed to ultraviolet irradiation for 1 h, the methyl orange decolorization ratio was 90%. When the load of CoFe2O4 in nanosized TiO2/expanded graphite reached 40%, its magnetic recovery efficiency reached 94.3%.